Fabrics & Upholstery · Furniture specification

Sekers Capella Faux Leather Furniture Specifications

A high-abrasion coated upholstery developed for contract seating where cleanability, repeatable colour and intensive use are priorities.

Current material reference

68.5% PVC, 1.5% PU, 15% PES, 15% cotton; 250,000 Martindale

Named supplier reference · current issue must be confirmed

Material decision summary

Project suitability at a glance.

Select the exact textile by end use, cleaning regime and verified test data; fibre content or abrasion alone is not enough.

Best for

  • +Intensive contract seating and food-and-beverage banquettes

Avoid when

  • A soft natural handle or breathable hide character is the main design intent
Traffic level
High
Maintenance
Low
Visual variation
Medium
Relative budget
●●○○
Suitable environments
Interior · High traffic · Food service

Material overview

Most requested furniture applications

Specify abrasion, cleaning method, flame performance, lightfastness, colourfastness, pilling, width and repeat according to the exact furniture location. “Contract grade” alone is not a complete specification.

Fabrics & Upholstery — Application view: completed contract chair
01 Application view: completed contract chair
01 Hotel lounge chairs and sofas
02 Restaurant dining chairs and banquettes
03 Guestroom headboards and benches

Material-specific authority schedule

Ten controls owned by this exact material—not inherited category rows. Final values are confirmed from supplier data, the project sample and shop drawings.

Sekers Capella Faux Leather Current material reference
01Sekers Capella Faux Leather
Osborne & Little Ariadne Velvet Current material reference
02Osborne & Little Ariadne Velvet
Declared project reference
Sekers Capella Faux Leather: 68.5% PVC, 1.5% PU, 15% PES, 15% cotton; 250,000 Martindale
Exact material identity
Project record: 68.5% PVC, 1.5% PU, 15% polyester, 15% cotton; 250,000 Martindale; exact current supplier issue still governs.
Technical system definition
A PVC/PU-coated upholstery composite on a textile backing. Its contract value depends on coating integrity, backing, flex and hydrolysis behaviour—not the leather-like face alone.
Selection differentiator
Very high recorded abrasion and wipeable coated face suit intensive banquettes when the complete upholstery build and cleaner are approved.
Critical approval decision
Verify that the exact CP36 colour and current backing/treatment retain the stated project abrasion performance and suit the project cleaner and fire route.
Non-equivalent substitute
A generic vinyl with similar grain is not equivalent without the same face/backing construction, flex, abrasion, colourfastness, fire route and cleaning compatibility.
Fabrication focus
Control coating stretch at tight radii, seam perforation, heat and adhesive contact; prototype the highest-tension corner.
GCC exposure limit
Confirm heat/humidity ageing and hydrolysis resistance for storage, transport and hot service zones before treating the abrasion figure as durability.
Material-specific care rule
Use only named approved cleaners and contact times; repeated disinfectant exposure can attack topcoat even when routine wiping appears safe.
Reject the delivery when
Reject cracking at folds, sticky surface, coating lift, dye transfer, seam tearing or lot mismatch.

Approval pack

Documents required before ordering.

Named supplier reference · current issue must be confirmed

  • Sekers Capella Faux Leather: Identity/source evidence: Project record: 68.5% PVC, 1.5% PU, 15% polyester, 15% cotton; 250,000 Martindale; exact current supplier issue still governs.
  • Sekers Capella Faux Leather: Signed selection evidence: Approve current tests for the supplied construction; do not translate Martindale textile cycles directly to coating life.
  • Sekers Capella Faux Leather: Second technical gate: Supplier confirms test conditions, result and warranty exclusions for the UAE service environment.
  • Sekers Capella Faux Leather: Factory close-out: Control coating stretch at tight radii, seam perforation, heat and adhesive contact; prototype the highest-tension corner.

Lead time & availability

Confirmed after source, finish and quantity selection

Family inspection atlas

A shared visual reference for construction and fabrication.

This atlas is shared by the material family; it is not a microscopy record of this exact selection. The approved sample and current supplier documents govern final colour and construction.

Sekers Capella Faux Leather — Surface macro: yarn, weave and fibre character
01 Surface macro: yarn, weave and fibre character
Sekers Capella Faux Leather — Construction edge: cover, seam, foam and frame
02 Construction edge: cover, seam, foam and frame
Sekers Capella Faux Leather — Workshop control: tailoring and seam execution
03 Workshop control: tailoring and seam execution
Sekers Capella Faux Leather — Application view: completed contract chair
04 Application view: completed contract chair

Material identity

What is unique—and what is shared with the family.

The exact material fingerprint comes first. Shared family science is explicitly separated in a collapsible appendix instead of being presented as unique content.

51 material-specific points · 39 shared family references

01 · Material fingerprint

What makes this exact selection technically distinct?

Position in the material family

Coated contract surface

Sekers Capella Faux Leather Current material reference
ASekers Capella Faux Leather · 68.5% PVC, 1.5% PU, 15% PES, 15% cotton; 250,000 Martindale
Fabrics & Upholstery — Surface macro: yarn, weave and fibre character
B Surface macro: yarn, weave and fibre character
Reference that must be declared
Project record: 68.5% PVC, 1.5% PU, 15% polyester, 15% cotton; 250,000 Martindale; exact current supplier issue still governs.
Selection differentiator
Very high recorded abrasion and wipeable coated face suit intensive banquettes when the complete upholstery build and cleaner are approved.
Not an equivalent substitute
A generic vinyl with similar grain is not equivalent without the same face/backing construction, flex, abrasion, colourfastness, fire route and cleaning compatibility.
Reject the delivery when
Reject cracking at folds, sticky surface, coating lift, dye transfer, seam tearing or lot mismatch.

Shared family reference

Open the shared Fabrics & Upholstery engineering appendix

This appendix applies to the complete Fabrics & Upholstery family. It is retained as supporting reference and is not counted as unique content for this material.

02 · System anatomy

The material is not a single surface.

A PVC/PU-coated upholstery composite on a textile backing. Its contract value depends on coating integrity, backing, flex and hydrolysis behaviour—not the leather-like face alone.

Fabrics & Upholstery — Construction edge: cover, seam, foam and frame
01 Construction edge: cover, seam, foam and frame
01 Wear face
02 Ground construction
03 Backing / treatment
04 Upholstery composite

01Wear face

Layer function

The visible fibre, pile or polymer film that receives abrasion, light, spills and cleaning.

How to verify

Declare fibre/polymer identity, colour, surface finish and exact tested article.

02Ground construction

Layer function

Woven, knitted or coated construction controls stretch, seam behaviour, drape and appearance retention.

How to verify

Record weave/knit/coating route, usable width, repeat and directional use.

03Backing / treatment

Layer function

Backing, FR treatment, stain finish or interliner can materially change hand, adhesion and fire behaviour.

How to verify

Approve the same backing and treatment represented in current test evidence.

04Upholstery composite

Layer function

Foam, interliner, adhesive, thread, seam and frame complete the performance system.

How to verify

Test and prototype the proposed cover/filling composite, not the loose textile alone.

03 · Decision gates

Reference benchmarks and the project rule.

Fabrics & Upholstery — Surface macro: yarn, weave and fibre character
V Surface macro: yarn, weave and fibre character

Abrasion

01
Reference band
General contract and high-traffic bands must use one stated method; ACT cites 40,000 Martindale cycles or 30,000 Wyzenbeek double rubs for high-traffic woven upholstery.
Project rule
Treat the result as comparative laboratory evidence, never a service-life promise.
Evidence status
Current report for exact article, colour and backing

Pilling

02
Reference band
ACT woven-upholstery reference: Class 3 minimum under ASTM D3511 or ASTM D4970.
Project rule
Increase the project requirement where a smooth appearance is critical.
Evidence status
Test report plus handled prototype

Seam slippage

03
Reference band
ACT woven-upholstery reference: 25 lbf minimum in warp and weft under ASTM D4034.
Project rule
Prototype curved corners, tight tailoring and high-load seams.
Evidence status
Laboratory result and seam sample

Light fastness

04
Reference band
ACT indoor woven reference: Grade 4 minimum at 40 hours under its cited AATCC routes; exterior exposure needs a separate outdoor route.
Project rule
Define window, atrium or exterior exposure rather than saying “colourfast”.
Evidence status
Exact-colour report and exposure location

Cleaning compatibility

05
Reference band
No universal number: record chemical name, dilution, contact time, rinse and frequency.
Project rule
Test the operator’s actual detergent/disinfectant on production material.
Evidence status
Written supplier compatibility and cleanability trial

Fire route

06
Reference band
Project and occupancy specific; results belong to the tested upholstery composite.
Project rule
State cover, treatment, interliner and filling represented by the certificate.
Evidence status
Current composite test evidence

04 · Family comparison

Four visually related systems that are not technically equivalent.

Sekers Capella Faux Leather Material alternative
01Sekers Capella Faux Leather
Osborne & Little Ariadne Velvet Material alternative
02Osborne & Little Ariadne Velvet
P Kaufmann Epiphany Polyurethane Material alternative
03P Kaufmann Epiphany Polyurethane
Casamance Reve de Burchell Woven Material alternative
04Casamance Reve de Burchell Woven
01 Current classification

Coated contract surface

Best use
F&B, healthcare-style cleaning and high-turnover seating where wipeability is central.
Trade-off / constraint
Hydrolysis, coating adhesion, heat and chemical compatibility must be verified.
02

Woven performance textile

Best use
General contract upholstery requiring comfort, texture and repairable tailoring.
Trade-off / constraint
Snagging, pilling, seam slippage and lot variation remain construction dependent.
03

Velvet / pile textile

Best use
Luxury guestrooms and controlled public areas where depth and light response matter.
Trade-off / constraint
Pile marking, pressure shading and cleaning skill are visible operational issues.
04

Solution-dyed outdoor textile

Best use
Pool, terrace and coastal cushions with a draining, quick-drying complete build-up.
Trade-off / constraint
Face-fabric performance cannot compensate for wet foam, trapped water or corroding hardware.

05 · Factory handbook

Hold points from receiving through production release.

Fabrication focus for this exact material

Control coating stretch at tight radii, seam perforation, heat and adhesive contact; prototype the highest-tension corner.

Fabrics & Upholstery — Workshop control: tailoring and seam execution
05 Workshop control: tailoring and seam execution
  1. 01Roll receiving

    Control instruction

    Record article, colour, dye lot, roll length, usable width, defects and face direction before acceptance.

    Close-out evidence

    Roll map, labels and photographed defect log

  2. 02Yield engineering

    Control instruction

    Nest furniture patterns using the approved nap, railroad direction, repeat and matching rule.

    Close-out evidence

    Cutting plan with net, repeat, waste and attic-stock quantities

  3. 03Seam prototype

    Control instruction

    Set needle, thread, stitch, seam allowance, backing and tension on the actual composite.

    Close-out evidence

    Signed high-stress seam and corner sample

  4. 04First-off upholstery

    Control instruction

    Review pattern placement, pile direction, seam grin, puckering, comfort interface and cleanability.

    Close-out evidence

    Approved first-off under project lighting

  5. 05Bulk release

    Control instruction

    Segregate lots, retain controls and prohibit silent backing/treatment substitutions.

    Close-out evidence

    Production traveller tied to control sample and lot

06 · Climate & operations

GCC exposure matrix and maintenance plan.

Material-specific climate warning

Confirm heat/humidity ageing and hydrolysis resistance for storage, transport and hot service zones before treating the abrasion figure as durability.

Fabrics & Upholstery — Application view: completed contract chair
06 Application view: completed contract chair

01Air-conditioned guestroom

Preferred
Material response
Generally stable, but window light and luggage abrasion remain local risks.
Design control
Select by item duty; protect window-adjacent colours and high-contact edges.

02High-turnover lobby

Conditional
Material response
Appearance change, pilling, seam load and cleaning frequency dominate.
Design control
Use contract evidence plus full-size first-off and replaceable detailing.

03Food & beverage

Conditional
Material response
Oils, coloured liquids and repeated chemical cleaning challenge the whole composite.
Design control
Approve stain/chemical trials and inaccessible-seam hygiene details.

04Direct sun / atrium

Conditional
Material response
Colour and polymer ageing accelerate; dark shades may heat strongly.
Design control
Require exact-colour light evidence and shade strategy.

05Pool / wet clothing

Avoid
Material response
Moisture, chlorine, sunscreen and slow drying create staining and microbial risk.
Design control
Use an approved outdoor composite with drainage, ventilation and cleanable seams.

06Coastal exterior

Avoid
Material response
UV, salt, humidity, windborne soil and wet foam act simultaneously.
Design control
Only purpose-designed exterior fabric, thread, foam, drainage and hardware qualify.

Operational maintenance plan

Material-specific care rule

Use only named approved cleaners and contact times; repeated disinfectant exposure can attack topcoat even when routine wiping appears safe.

  1. 01Each service / daily

    Action

    Vacuum or brush loose soil in the approved direction; blot fresh spills immediately.

    Prohibited

    Do not rub a wet stain or flood seams.

  2. 02After a spill

    Action

    Identify soil, use the approved dilution and work from edge to centre; rinse only if instructed.

    Prohibited

    No unlisted solvent, bleach or heat.

  3. 03Monthly

    Action

    Inspect high-contact fronts, piping, corners, seams, pile direction and concealed moisture.

    Prohibited

    Do not wait for foam or backing damage to become visible.

  4. 04Periodic deep clean

    Action

    Use the supplier-approved professional method and dry the composite completely before service.

    Prohibited

    No generic extraction method without backing/foam approval.

  5. 05Repair / replacement

    Action

    Use retained same-lot stock where possible; record replacement lot and panel position.

    Prohibited

    Do not mix a visibly different lot across one furniture face.

07 · Reference library

The language that governs the decision—and where it comes from.

Fabrics & Upholstery — Surface macro: yarn, weave and fibre character
01 Surface macro: yarn, weave and fibre character
Fabrics & Upholstery — Construction edge: cover, seam, foam and frame
02 Construction edge: cover, seam, foam and frame
Fabrics & Upholstery — Workshop control: tailoring and seam execution
03 Workshop control: tailoring and seam execution
Fabrics & Upholstery — Application view: completed contract chair
04 Application view: completed contract chair

Material glossary

01Martindale
A laboratory abrasion method; the cycle result is method-specific and does not predict years of service.
02Wyzenbeek
A reciprocating abrasion method reported in double rubs; it is not numerically interchangeable with Martindale.
03Railroaded
The pattern or construction can be used across the roll width, affecting seams and yield.
04Crocking
Transfer of colour from the textile by dry or wet rubbing.
05Dye lot
A production batch expected to have closer colour continuity than separately dyed batches.

Professional and standards sources

  1. 01

    ACT

    Woven upholstery performance guidelines

    Voluntary reference bands for abrasion, pilling, strength, seams and colourfastness.

    Open primary source ↗
  2. 02

    ISO

    ISO 12947-2 Martindale abrasion

    Specimen breakdown determination for textile fabrics.

    Open primary source ↗
  3. 03

    ISO

    ISO 105-X12 rubbing fastness

    Dry and wet rubbing colour-transfer method.

    Open primary source ↗
  4. 04

    BSI

    BS 7176 non-domestic seating

    Ignition-resistance classification through tested upholstery composites.

    Open primary source ↗

Material-specific technical dossier

Sekers Capella Faux Leather controls from decision to production.

Every row below is tied to this material’s identity, differentiator, fabrication, exposure or care route; no generic family rows are included in this dossier.

8 unique controls · 5 contextual test applications · 5 material-specific risks

System definition

A PVC/PU-coated upholstery composite on a textile backing. Its contract value depends on coating integrity, backing, flex and hydrolysis behaviour—not the leather-like face alone.

Critical decision

Verify that the exact CP36 colour and current backing/treatment retain the stated project abrasion performance and suit the project cleaner and fire route.

01 · Selection variables

What the material schedule must lock.

Sekers Capella Faux Leather Current material reference
68.5% PVC, 1.5% PU, 15% PES, 15% cotton; 250,000 Martindale

01Sekers Capella Faux Leather: Coated-face durability

What must be declared
Wet/dry coated-fabric abrasion, flex cracking, coating adhesion and cold/heat response
Approval basis
Approve current tests for the supplied construction; do not translate Martindale textile cycles directly to coating life.

02Sekers Capella Faux Leather: Hydrolysis & cleaner resistance

What must be declared
Humidity ageing plus named detergent/disinfectant contact
Approval basis
Supplier confirms test conditions, result and warranty exclusions for the UAE service environment.

03Sekers Capella Faux Leather: identity declaration

What must be declared
Project record: 68.5% PVC, 1.5% PU, 15% polyester, 15% cotton; 250,000 Martindale; exact current supplier issue still governs.
Approval basis
Verify that the exact CP36 colour and current backing/treatment retain the stated project abrasion performance and suit the project cleaner and fire route.

04Sekers Capella Faux Leather: equivalency boundary

What must be declared
Very high recorded abrasion and wipeable coated face suit intensive banquettes when the complete upholstery build and cleaner are approved.
Approval basis
A generic vinyl with similar grain is not equivalent without the same face/backing construction, flex, abrasion, colourfastness, fire route and cleaning compatibility.

05Sekers Capella Faux Leather: factory execution

What must be declared
Control coating stretch at tight radii, seam perforation, heat and adhesive contact; prototype the highest-tension corner.
Approval basis
Approve current tests for the supplied construction; do not translate Martindale textile cycles directly to coating life.

06Sekers Capella Faux Leather: GCC exposure control

What must be declared
Confirm heat/humidity ageing and hydrolysis resistance for storage, transport and hot service zones before treating the abrasion figure as durability.
Approval basis
Release only when the project detail and maintenance route close this exact exposure risk for Sekers Capella Faux Leather.

07Sekers Capella Faux Leather: operational care route

What must be declared
Use only named approved cleaners and contact times; repeated disinfectant exposure can attack topcoat even when routine wiping appears safe.
Approval basis
Issue a named cleaning and repair method for Sekers Capella Faux Leather; generic family care is not approval.

08Sekers Capella Faux Leather: delivery rejection boundary

What must be declared
Reject cracking at folds, sticky surface, coating lift, dye transfer, seam tearing or lot mismatch.
Approval basis
The signed sample, first-off item and delivery inspection must all close this rejection condition for Sekers Capella Faux Leather.

02 · Verification

Test and evidence matrix.

Test methods are not compliance certificates or automatic pass values. The project must state the method, required result, tested construction and current report it will accept.

Fabrics & Upholstery — Construction edge: cover, seam, foam and frame
02 Construction edge: cover, seam, foam and frame

ISO 12947-2 / ISO 12947-4

01
What it measures
Martindale specimen breakdown and appearance change for uncoated textiles.
How to use it here
Specify the applicable part and project acceptance level; a cycle count is not a universal service-life guarantee. Material-specific acceptance for Sekers Capella Faux Leather: Approve current tests for the supplied construction; do not translate Martindale textile cycles directly to coating life.
Official reference ↗

ISO 5470-2

02
What it measures
Wet and dry abrasion of rubber- or plastics-coated fabric surfaces.
How to use it here
Use for coated faux leather/PU faces where ISO 12947 for uncoated textiles is not the correct surface method. Material-specific acceptance for Sekers Capella Faux Leather: Supplier confirms test conditions, result and warranty exclusions for the UAE service environment.
Official reference ↗

ISO 105-X12

03
What it measures
Colour transfer and staining under dry and wet rubbing.
How to use it here
Test the exact colour; dark and saturated shades can behave differently from collection averages. Material-specific acceptance for Sekers Capella Faux Leather: Require ageing/cleaner evidence and validate the exact operations chemical on production material.
Official reference ↗

ISO 105-B02

04
What it measures
Colour fastness to artificial light representative of daylight.
How to use it here
Prioritise for window-adjacent, atrium and exterior applications; state the required rating. Material-specific acceptance for Sekers Capella Faux Leather: Control coating stretch at tight radii, seam perforation, heat and adhesive contact; prototype the highest-tension corner.
Official reference ↗

BS EN 1021-1 / BS 7176

05
What it measures
Ignitability of upholstery composites and non-domestic seating hazard classification.
How to use it here
The project fire strategy determines the route. Submit evidence for the actual cover/filling composite. Material-specific acceptance for Sekers Capella Faux Leather: Confirm heat/humidity ageing and hydrolysis resistance for storage, transport and hot service zones before treating the abrasion figure as durability.
Official reference ↗

03 · Performance

Failure-mode and control register.

Sekers Capella Faux Leather applied to its dedicated furniture product
Sekers Capella Faux Leather applied to its dedicated furniture product

01Sekers Capella Faux Leather: Surface peeling or sticky breakdown

Likely cause
Coating hydrolysis, plasticiser migration or incompatible cleaner under heat/humidity.
Preventive control
Require ageing/cleaner evidence and validate the exact operations chemical on production material.

02Sekers Capella Faux Leather: non-equivalent substitution accepted

Likely cause
A generic vinyl with similar grain is not equivalent without the same face/backing construction, flex, abrasion, colourfastness, fire route and cleaning compatibility.
Preventive control
Project record: 68.5% PVC, 1.5% PU, 15% polyester, 15% cotton; 250,000 Martindale; exact current supplier issue still governs.

03Sekers Capella Faux Leather: material signature lost in fabrication

Likely cause
The workshop route does not implement the material-specific fabrication focus: Control coating stretch at tight radii, seam perforation, heat and adhesive contact; prototype the highest-tension corner.
Preventive control
Supplier confirms test conditions, result and warranty exclusions for the UAE service environment.

04Sekers Capella Faux Leather: GCC exposure mismatch

Likely cause
Confirm heat/humidity ageing and hydrolysis resistance for storage, transport and hot service zones before treating the abrasion figure as durability.
Preventive control
Re-detail, relocate or reject Sekers Capella Faux Leather where the stated exposure cannot be controlled.

05Sekers Capella Faux Leather: cleaning or maintenance damage

Likely cause
Use only named approved cleaners and contact times; repeated disinfectant exposure can attack topcoat even when routine wiping appears safe.
Preventive control
Train operations on the named care route and retain a signed repair reference for Sekers Capella Faux Leather.

04 · Tender-ready

Copy-ready specification clause.

Provide Sekers Capella CP36 or approved equivalent coated upholstery, project reference composition 68.5% PVC, 1.5% PU, 15% polyester and 15% cotton, subject to confirmation by the current manufacturer data sheet for the selected colour. Submit coating/backing construction, usable width and weight, wet/dry coated-face abrasion, flex and hydrolysis/ageing evidence, dry/wet rub fastness, cleaning compatibility and fire evidence for the proposed upholstery composite. Approval requires a current dye-lot cutting and first upholstered prototype; a similar colour or unverified Martindale claim is not equivalent.

05 · Quality control

Inspection plan from submittal to handover.

Fabrics & Upholstery — Workshop control: tailoring and seam execution
05 Workshop control: tailoring and seam execution

01Sekers Capella Faux Leather: identity and source

Inspection
Project record: 68.5% PVC, 1.5% PU, 15% polyester, 15% cotton; 250,000 Martindale; exact current supplier issue still governs.
Acceptance / hold point
Documents, labels and physical material all identify the same Sekers Capella Faux Leather construction and source.

02Sekers Capella Faux Leather: control sample

Inspection
Very high recorded abrasion and wipeable coated face suit intensive banquettes when the complete upholstery build and cleaner are approved.
Acceptance / hold point
Approve current tests for the supplied construction; do not translate Martindale textile cycles directly to coating life.

03Sekers Capella Faux Leather: first-off fabrication

Inspection
Control coating stretch at tight radii, seam perforation, heat and adhesive contact; prototype the highest-tension corner.
Acceptance / hold point
Supplier confirms test conditions, result and warranty exclusions for the UAE service environment.

04Sekers Capella Faux Leather: exposure and care trial

Inspection
Confirm heat/humidity ageing and hydrolysis resistance for storage, transport and hot service zones before treating the abrasion figure as durability. Use only named approved cleaners and contact times; repeated disinfectant exposure can attack topcoat even when routine wiping appears safe.
Acceptance / hold point
Require ageing/cleaner evidence and validate the exact operations chemical on production material.

05Sekers Capella Faux Leather: delivery release

Inspection
Reject cracking at folds, sticky surface, coating lift, dye transfer, seam tearing or lot mismatch.
Acceptance / hold point
Sekers Capella Faux Leather is released only when no stated rejection condition is present and the signed reference remains traceable.

Required approval evidence

  • +Sekers Capella Faux Leather: Identity/source evidence: Project record: 68.5% PVC, 1.5% PU, 15% polyester, 15% cotton; 250,000 Martindale; exact current supplier issue still governs.
  • +Sekers Capella Faux Leather: Signed selection evidence: Approve current tests for the supplied construction; do not translate Martindale textile cycles directly to coating life.
  • +Sekers Capella Faux Leather: Second technical gate: Supplier confirms test conditions, result and warranty exclusions for the UAE service environment.
  • +Sekers Capella Faux Leather: Factory close-out: Control coating stretch at tight radii, seam perforation, heat and adhesive contact; prototype the highest-tension corner.
  • +Sekers Capella Faux Leather: Exposure and care record: Confirm heat/humidity ageing and hydrolysis resistance for storage, transport and hot service zones before treating the abrasion figure as durability. Use only named approved cleaners and contact times; repeated disinfectant exposure can attack topcoat even when routine wiping appears safe.
  • +Sekers Capella Faux Leather: Delivery rejection record: Reject cracking at folds, sticky surface, coating lift, dye transfer, seam tearing or lot mismatch.

Questions to close before approval

  1. 01Sekers Capella Faux Leather: Has the exact identity been declared and evidenced: Project record: 68.5% PVC, 1.5% PU, 15% polyester, 15% cotton; 250,000 Martindale; exact current supplier issue still governs?
  2. 02Sekers Capella Faux Leather: Which project requirement makes this differentiator necessary: Very high recorded abrasion and wipeable coated face suit intensive banquettes when the complete upholstery build and cleaner are approved?
  3. 03Sekers Capella Faux Leather: Has the team excluded the non-equivalent route: A generic vinyl with similar grain is not equivalent without the same face/backing construction, flex, abrasion, colourfastness, fire route and cleaning compatibility?
  4. 04Sekers Capella Faux Leather: How will the factory prove this execution control: Control coating stretch at tight radii, seam perforation, heat and adhesive contact; prototype the highest-tension corner?
  5. 05Sekers Capella Faux Leather: Can the project control this GCC exposure: Confirm heat/humidity ageing and hydrolysis resistance for storage, transport and hot service zones before treating the abrasion figure as durability?
  6. 06Sekers Capella Faux Leather: Who owns this operating rule after handover: Use only named approved cleaners and contact times; repeated disinfectant exposure can attack topcoat even when routine wiping appears safe?

Exact material application

Sekers Capella Faux Leather on a dedicated furniture product.

This material-specific application image shows Sekers Capella Faux Leather on its own product and is not reused by any other material page. Final colour, pattern and finish remain subject to the approved physical sample.

Sekers Capella Faux Leather applied to its dedicated furniture product
01Sekers Capella Faux Leather applied to its dedicated furniture product

Project notes

From sample to production.

01

What to specify

Specify abrasion, cleaning method, flame performance, lightfastness, colourfastness, pilling, width and repeat according to the exact furniture location. “Contract grade” alone is not a complete specification.

02

Fabrication & detailing

Confirm repeat, direction, seam placement, FR interliner and foam compatibility before cutting. High-contact furniture should use replaceable covers or serviceable upholstery details where practical.

03

Colour & finish approval

Colour, texture, pile direction and dye-lot variation are approved from a current cutting. Pattern alignment and railroad suitability are checked against the furniture drawing.

04

Care & maintenance

Vacuum gently and blot spills immediately. Use only the cleaning method approved for the selected fibre and finish; test any agent on a concealed sample first.

Specification note

This page is a preliminary specification guide. No value, brand reference or material name constitutes automatic compliance. Current product data, test reports, physical sample or slab and the furniture construction must be approved for each project before ordering or manufacture.

Request an approval sample for Sekers Capella Faux Leather

Share the material schedule, furniture item, quantity and project location. We will confirm the sample, furniture construction and technical documents required for approval.